Poly[N-isopropylacrylamide-co-4-(diphenylphosphino)styrene] Palladium(II) Dichloride (ratio, acrylamide:phosphine=20:2)


Purity:
Synonyms:
  • Palladium Catalyst, supported with Poly[N-isopropylacrylamide-co-4-(diphenylphosphino)styrene] (ratio, acrylamide:phosphine=20:2)
Product Documents:
100MG
$180.00
3   Contact Us 7  

* Items in stock locally ship in 1-2 business days. Items from Japan stock are able to ship from a US warehouse within 2 weeks. Please contact TCI for lead times on items not in stock. Excludes regulated items and items that ship on ice.
* To send your quote request for bulk quantities, please click on the "Request Quote" button. Please note that we cannot offer bulk quantities for some products.
*TCI frequently reviews storage conditions to optimize them. Please note that the latest information on the storage temperature for the products is described on our website.


Product Number P1425
Physical State (20 deg.C) Solid
Storage Temperature Room Temperature (Recommended in a cool and dark place, <15°C)
Store Under Inert Gas Store under inert gas
Condition to Avoid Air Sensitive
PubChem Substance ID 87575500
MDL Number

MFCD04041046

Specifications
Appearance Black powder to crystal
Functionality test to pass test
NMR confirm to structure
Properties (reference)
GHS
Related Laws:
Transport Information:
HS Number 2931.90.6000
Application
Reusable Amphiphilic Polymer-assembled Pd Complex Catalyst

Typical procedure : Recycling of Pd complex catalyst for the Suzuki-Miyaura reaction.
(X = I, R1 = R3 = H) : A mixture of phenyl iodide (4.59 g, 22.5 mmol), phenylboronic acid (3.00 g, 24.8 mmol), and Na2CO3 (2.65 g, 25.0 mmol) in water (75 mL) is degassed by ultrasonication for 30 min. To the solution is added amphiphilic polymer-assembled Pd complex catalyst (3.40 mg, 5.0 x 10-3 mol%), and the resulting suspension is stirred at 100 °C for 24 h. After the reaction, the mixture is filtered with hot water, the glass filter is washed with hot water. At that time, the Pd complex catalyst is recovered on the filter. The filtrate is cooled to room temperature to afford crystals. It is isolated on the filter and dried in vacuo to give biphenyl. The recovered Pd complex catalyst is dried in vacuo and reused.

References


Product Documents (Note: Some products will not have analytical charts available.)
Safety Data Sheet (SDS)
Please select Language.

The requested SDS is not available.

Please Contact Us for more information.

Specifications
C of A & Other Certificates
Please enter Lot Number Incorrect Lot Number. Please input only the 4-5 alphanumeric characters before the hyphen.

The product with the lot number searched for has been discontinued and no related documentation is available.

Sample C of A
This is a sample C of A and may not represent a recently manufactured lot of the product.

A sample C of A for this product is not available at this time.

Analytical Charts
Please enter Lot Number Incorrect Lot Number. Please input only the 4-5 alphanumeric characters before the hyphen.

The requested analytical chart is not available. Sorry for the inconvenience.

The product with the lot number searched for has been discontinued and no related documentation is available.

Other Documents

Session Status
Your session will timeout in 10 minutes. You will be redirected to the HOME page after session timeout. Please click the button to continue session from the same page. minute. You will be redirected to the HOME page after session timeout. Please click the button to continue session from the same page.

Your session has timed out. You will be redirected to the HOME page.